HT-Mn75 manganese agent

7*24 hours free consultation telephone

+86-0516-83246699

60-second manual response

Give technical consultation reply within 30 minutes

Free solution design for 24 hours

product description

technical parameter

HT-Mn75 manganese agent

1. Purpose:

Adjust the content of manganese in different grades of aluminum alloy to replace the master alloy and reduce the melting temperature.

2. Product features:

1. The element content is 75%

2. The actual yield is greater than 95%

3. Direct investment, easy to use.

3. How to use:

According to the content of alloying elements in the alloy grades produced and the results of the pre-furnace analysis, the required additive amount (quantity of Mn agent) is calculated according to the actual yield of 90%. After the small flame disappears, manual stirring should be appropriately strengthened to make it spread evenly, and according to the actual situation, ensure a certain spread time.

4. Process parameters:

1. Operating temperature: 740-760℃

2. Addition amount (kg) = (alloy element composition (%)-analysis of the element content before the furnace) ÷ actual yield (90%) × alloy element content in the additive (70%) × furnace load (kg)

3. Melting time: 15-30 minutes

5. Packaging and storage:

Product name

model

use

Instructions

Features

Process parameters

specification

HT-Ti

HT-Ti4OB4

Adjust the alloying element composition to replace the aluminum master alloy.

According to the content of alloying elements in the produced alloy grades and the results of the pre-furnace analysis, the actual yield is calculated at 95%. The required additive amount is directly and evenly dispersed into the aluminum bath after the slag is removed, and the small flame disappears After that, manual stirring should be appropriately strengthened to make the diffusion even, and according to the actual situation, ensure a certain diffusion time.


The element content is 75% and the silicon content is 95%.

The actual yield is greater than 95%.

The actual yield of iron agent is greater than 90%.

The shelf life is one year.



Operating temperature: 740℃-760℃.

Melting time: 15-30 minutes.



1.500g/piece

Density: 3.8-4.2kg/cm3

Si: 2.5g/cm3


HT-Ti

HT-Ti75

HT-Mn

HT-Mn75

HT-Cu

HT-Cu75

HT-Fe

HT-Fe75

HT-Cr

HT-Cr75

HT-Ni

HT-Ni75

HT-Zn

HT-Zn75

HT-Si

HT-Si95

Online consultation

If you are interested in our products, or if we can help you, you can always call our national customer service number:+86-0516-83246699

You can also communicate with us online, of course, you can also leave us a message below, we will be happy to serve you!

Contact us

Customer first, thoughtful service, superior quality, technological quality

  • Address: Wushao Industrial Zone, Zhangji Town, Xuzhou City, Jiangsu Province

    Phone: +86-0516-83246699

    Fax: +86-0516-83246555

    Email: sales@xzyhjs.com

    Website: http://ynzbt.com


  • 2020 All Rights Reserved ?Xuzhou Yuhao Nonferrous Metal Material Co., Ltd.